Fig 4

Fig. 4: Isotherm analysis at 150 °C coupled with gas analysis of a 25µm thick ZrO2 layer formed onto Zr4 fuel cladding (350°C, 155 bars) after 3500 hours of pool immersion. The graph shows water (green) and hydrogen (black) release rates, and cumulated global cladding mass loss (red) in arbitrary units (a.u.) as function of temperature (blue) and time.


Back to Feature Details



Privacy Policy
We have updated our privacy policy. In the latest update it explains what cookies are and how we use them on our site. To learn more about cookies and their benefits, please view our privacy policy. Please be aware that parts of this site will not function correctly if you disable cookies. By continuing to use this site, you consent to our use of cookies in accordance with our privacy policy unless you have disabled them.